VCR Face Seal Fittings: Inspection and Installation Checks

Quick answer. A metal gasket face seal joint — sold under the trade name VCR, a Swagelok trademark used generically in the industry — is made by two polished circular shoulders pressing a metal gasket between them. The parts are a long or short gland on each side, a male nut and a female nut, and one gasket in the middle. Nothing about the seal is adjustable at the bench: if the shoulders are clean and the gasket is seated correctly, the joint closes; if a shoulder is scratched or the gasket is off its seat, no amount of tightening will help. That is why the inspection list below matters more than the wrench.

The four parts of a face seal joint: long gland, male nut, metal gasket, female nut and short gland — the shoulders are the sealing faces
The four parts of a face seal joint: long gland, male nut, metal gasket, female nut and short gland — the shoulders are the sealing faces

The four parts, and what each one does

PartRole
Long gland / short glandWeld into the tube end. Carries the polished circular shoulder that forms one half of the seal.
Male nutThreads onto the gland and presents the mating shoulder.
Metal gasketThe sealing element. Compressed between the two shoulders; replaced at every make-up.
Female nutInternally threaded; pulls the two shoulders together. Silver plated for easier assembly, consistent make-up, galling resistance and lower assembly torque.

The catalog covers 1/8″ to 1″ tube sizes in SS316L.

Brand note. “VCR” is a trademark of Swagelok Company and is widely used across the industry as the generic name for this fitting family. PC Vacuum supplies metal gasket face seal fittings to this construction; brand names appear here only to describe the product category.

The sealing principle in one line

Both gland ends finish in a highly polished circular shoulder. When the female and male nuts are tightened, those two shoulders come face to face and compress the gasket between them. The seal is metal-to-metal at the gasket, not a polymer compression — which is why a scratch on a shoulder is fatal and why the gasket is a single-use part.

Inspect before you assemble

This is the check list that decides whether the joint will hold:

#CheckWhat to look for
1Gland shouldersA polished circular face at each gland end. Look for scratches, dings, burrs or embedded debris under good light — each one is a potential leak path.
2GasketCorrect size for the tube O.D., sitting square and flat on the male shoulder. Confirm it is not missing, not dropped into the nut body and not off-centre.
3ThreadsClean, undamaged threads on both nuts and both glands. Grit or a crossed start shows up later as a make-up torque that feels wrong.
4PlatingThe female nut’s silver plating eases assembly and resists galling. Do not wire-brush it off, and do not substitute an unplated nut where a plated one is specified.
5AlignmentStart the nut by hand and bring it down square. Cross-threading starts here, not at the wrench.

Two of these are worth repeating because they account for most field failures: a reused gasket and a gasket that never sat on the shoulder. In both cases the joint closes, feels tight, and leaks.

Two polished shoulders press the metal gasket. The inspection list before assembly matters more than the wrench: a scratched shoulder or an off-seat gasket closes tight and still leaks
Two polished shoulders press the metal gasket. The inspection list before assembly matters more than the wrench: a scratched shoulder or an off-seat gasket closes tight and still leaks

The make-up sequence

  1. Seat the gasket on the male shoulder. It should sit flat and stay there on its own.
  2. Bring the female nut down by hand, keeping it square to the threads.
  3. Hand-tighten until the two shoulders meet the gasket. The joint is now closed mechanically — everything after this is confirming, not creating, the seal.
  4. Wrench to make-up, according to the assembly procedure your line follows. The shoulders bottom out on the gasket; torque past that point deforms the nut and the shoulder instead of improving the seal.

Why the gasket is replaced every time

The shoulder impresses the gasket at every make-up: the gasket is the soft part of the pair and it takes the shape of the joint. A gasket that has already been seated has an impression in it, and it will not seat reliably a second time. Treat a gasket as one per joint, per assembly — and treat any joint you open for inspection as a joint that needs a new gasket before it goes back into service.

That has a practical consequence for layout: a face seal joint is not something you can break and re-close to check whether the fit is right. Get the geometry right on the drawing, not by test assemblies.

Choose size and wall first — the pressure table is indexed by both

Tube O.D.Wall thicknesspsibar
1/8″0.028″ (0.71 mm)8550590
1/4″0.035″ (0.89 mm)5200359
3/8″0.035″ (0.89 mm)3350231
1/2″0.049″ (1.24 mm)3750259
3/4″0.065″ (1.65 mm)2400165
1″0.065″ (1.65 mm)2400165

Values are quoted per row from the catalog table. The rating depends on the tube size, wall thickness, material, gasket and assembly conditions together: the highest value in the table belongs to the 1/8″ row and is not a system-wide rating. Confirm the figure for your exact combination at quotation.

Surface finish: BA or EP

FinishRa rangeTypical reason to select it
BA (bright annealed)0.4–1.0 μmStandard high-purity duty.
EP (electropolished)0.13–0.25 μmWhere the lowest surface roughness is required by the line’s specification.

Finish follows the purity requirement of the gas or vacuum line. It is a specification choice made when the fitting is ordered, not something modified afterwards.

Where these joints are used

High-purity gas delivery, semiconductor process gas lines and clean vacuum interfaces — anywhere an all-metal, low-particulate joint is required at small bore. For the larger all-metal system, the CF flange family closes on a knife edge and copper gasket, and the rotatable vs fixed CF flange comparison covers the hole patterns and alignment rules. Where an elastomer joint suits the duty, KF fittings and the three-system overview in KF vs ISO vs CF set out the alternatives. Valve and manifold ends follow the same face seal rules as any other joint in the run — see Vacuum Valves for the connection options.

What to send with the enquiry

#Item
1Tube O.D. and wall thickness
2Components required: long gland, short gland, male nut, female nut, gaskets
3Surface finish: BA or EP
4Material (SS316L in the catalog)
5Medium and purity requirement
6Pressure and temperature duty, plus any bake requirement
7Quantity, and whether gaskets should be supplied as spare sets

Send your specification

Frequently asked questions

Can a face seal gasket be reused if the joint was never pressurised?

The shoulder impresses the gasket as soon as the joint is made up, so a gasket that has been seated once is replaced before the joint goes back into service. Plan one gasket per joint per assembly.

Is “VCR” your brand?

No. VCR is a trademark of Swagelok Company, widely used in the industry as the generic name for this fitting family. We supply fittings to the same construction, ordered by dimensions, material and finish.

Why is the female nut silver plated?

For easier and more consistent assembly, resistance to galling and lower make-up torque. The plating is part of the part — it is not removed or replaced at assembly.

Does the make-up torque depend on the size?

The catalog pressure table is indexed by tube O.D. and wall thickness, which shows how much the geometry changes across the 1/8″ to 1″ range. Follow the make-up procedure that applies to your size and joint.

BA or EP — which finish should I choose?

EP where the line specifies the lowest surface roughness (0.13–0.25 μm); BA (0.4–1.0 μm) otherwise. Confirm against the purity specification of the line.

What pressure can these fittings take?

The catalog lists a pressure value per tube size and wall thickness, from 8550 psi at 1/8″ to 2400 psi at 3/4″ and 1″. The applicable rating for your combination is confirmed at quotation — the values are not interchangeable between sizes.

Where does the leak test happen?

The catalog describes visual inspection and leak testing through two ports at opposite positions of the fitting. The method and acceptance criteria for your order are confirmed with the quotation.

Scroll to Top

Get a Quote